Weld cleaning brush made for use on 4.5-in. grinders

February 19, 2013

Weld cleaning brush made for use on 4.5-in. grinders - TheFabricator.com

Weiler Corp.'s 4.5-in. Roughneck® weld cleaning brush is designed for use on 4.5-in. grinders. It features a high knot count and short trim length, which the company says results in a 35 percent improvement in cleaning action, up to 20 percent less wire loss, and 50 percent longer brush life than a comparable 4-in. stringer bead brush.

The weld cleaning brush is available in both carbon steel and Type 302 stainless steel wire with a variety of arbor hole options.