June 13, 2006
American Torch Tip has developed an antireflection coating for its focusing lenses.
The coating achieves absorption rates as low as 18 percent, allowing the lens to retain less heat for cool running and extended life.
The coating is available in Plano Convex and Meniscus styles and in many diameters and thicknesses.