Pemamek offers the Pema CM 55 milling machine for joint preparation of circumferential seams. According to the company, the machine increases welding quality and efficiency, with features designed to help reduce the defect rate.

The unit offers precise groove preparation and root opening even in thick walls. The milling depth can be up to 5.5 in. while providing 55-kW spindle power. The depth control is equipped with servo slide and sensor feedback.

The unit is equipped with lifting points that enable easy moving. The main frame is supported and leveled with hydraulic legs.