Stainless steel product line expanded


February 7, 2014

Rolled Alloys has announced the expansion of its 17-4 stainless steel product line, including rounds, plate, and welding consumables.

The company now offers the round bar in sizes from 0.1875 to 12 in. dia. in standard lengths or cut to size. Multiple heat-treatment conditions also are available.