The ALFA oxyfuel torch from MG Systems and Welding has completely integrated height sensing and internal auto-ignition, eliminating external parts that can become coated in slag or become damaged by tip ups or other working hazards.

Able to sense right up to the plate edge, the torch isn't affected by slag, mill scale, or moisture. Changing consumables requires no tools.

Fully automated oxyfuel cutting is provided when the torch is paired with the company's OmniFlow gas control system.