November 11, 2008
Victor Equipment Co. now offers a series of cutting, welding, and heating torches and outfits.
The Performer® is the lightest outfit in the series and can weld from 1/32 in. to 1-1/4 in. and cut 1/8 in. to 6 in. The SuperRange® II is a medium-duty outfit suitable for cutting and heating with on a daily basis. The torch is similar to the light outfit, but comes with larger 350 series regulators and gauge guards and is designed for use on medium to medium-heavy applications.
The Contender® is a heavy-duty outfit that includes a CA 2460 cutting attachment, a 315FC handle, 350 regulators with gauge guards, a 25-ft. T-grade hose, a 1-1-101 cutting tip, a #6 MFA, a striker, and a professional toolbox. It features built-in check valves and flashback arresters.
The Journeyman® and Journeyman II, when used with the appropriate tips, weld between 1/32 in. and 3 in. and cut from 1/8 in. to 8 in. The heavy-duty outfit cuts, welds, and heats. It is suitable for cutting steel on a daily basis.
Products in Oxyfuel Cutting |