July 10, 2007
Hypertherm Inc. has released 50-amp cutting consumables designed to optimize operation when cutting mild steel with thickness between 22 ga. and 5/16 in.
The consumables are available for the HyPerformance Plasma® HPR130 and HPR260 systems, as well as for the HyDefinition® HD3070 and HD4070 systems retrofitted with a HyPerformance Plasma torch.
In addition to the 30- 50-, and 80-amp power levels, the company offers consumables at 100, 130, 200, and 260 amps.
Hypertherm Inc. * 800-643-0030 * www.hypertherm.com