February 28, 2013

Retro Systems has launched the Mega Hornet 1000 floor-mounted rail cutting machine. It is the third model in the series of machines equipped with multiple tool carriages supporting the plasma and oxyfuel cutting processes.

Constructed from a welded and stress-relieved gantry beam and fabricated steel end trucks, the CNC system offers spans up to 14 ft. and features up to six cutting and marking carriages. The machine incorporates AC servo amplifiers and servomotors; precision planetary gearboxes; precision-ground, cross-axis linear ways; and a heavy-duty, machined, floor-mounted rail system.