American Torch Tip Co. has released a full line of high-definition electrodes for use in high-amperage plasma applications.
The series is manufactured to hold tolerances to within ± 0.0005 in. for critical tolerances, providing consistent cut quality and extended electrode life. The replacement series is available for Hypertherm®, Komatsu®, Innerlogic®, and ESAB® torches.