The FABRICATORSTAMPING JournalPractical Welding TodayTube & Pipe Journalthefabricator.comCanadian Industry ManufacturingGreen ManufacturerPWT TVTPJ TV

 
Plasma Cutting Product News
Home \ Plasma Cutting \ Products \ Oxygen plasma system introduced

Oxygen plasma system introduced

May 8, 2007

Hypertherm Inc. has announced the release of HySpeed Plasma HSD130, a easy-to-use, mechanized, oxygen plasma system.

The system includes the company's patented LongLife® technology, designed to deliver double the consumable life at half the cost, the company says.

Recommended for small- to medium-sized companies, the system cuts dross-free at 5/8 in. (16mm) on mild steel. Production pierce capability is 1 in. (25mm), with maximum cutting at 1 in. (38mm).