Hypertherm has introduced a new Centricut brand quick-change torch for use with ESAB plasma cutting systems. The torch is designed to replace ESAB PT-36, PT-600, and PT-19XLS torches.

According to the company, the two-piece, quick-change design allows operators to change out consumables up to three times faster, or, with the use of multiple torch heads, to load consumables for the next job while cutting the current job.

The company says that its SilverLine electrode features a hybrid copper/silver weld joint that delivers performance equal to a solid silver electrode at a lower cost. CoolFlow technology improves cooling to help maintain the size and shape of the nozzle orifice.