The M.K. Morse Co. has introduced the Morse 811, a portable band saw blade. It is designed for cutting a variety of sizes and types of materials with a single blade.

The patent-pending blade combines an aggressive tooth with a variable tooth pattern to help reduce vibration and increase cutting speed. The tooth tips are made of high-speed steel. The blade is 0.5 in. wide and 0.020 in. thick. It comes in various blade sizes for corded and cordless portable band saws from 27.1875 to 44.875 in.