Carbide band saw blade coated to prevent heat buildup


September 10, 2013

LENOX® offers the LENOX ARMOR CT BLACK® carbide band saw blade. The coating comprises aluminum, titanium, and nitrogen to protect each tooth from heat and wear.

The blade features backing steel is heat-treated and prepared to help minimize premature band breaks. With its micrograined carbide tips, the blade can cut a variety of metals, including carbon steels, mold steels, alloy steels, tool steels, bearing steels, stainless steels, structural steels, and titanium alloys.