System automates compound mitering process


November 6, 2013

System automates compound mitering process - TheFabricator.com

TigerStop has introduced the TigerAngle automated compound mitering and length-positioning system. It is designed for applications requiring high-volume horizontal- and vertical-angle cutting.

The system can be used solely as a stop in a set-point operation or as a push-feed operation. It eliminates manual adjustment of the saw to the proper miter angles, as well as the setting of stops.