Vertical-airflow cabinet oven developed

Grieve has developed No. 814, a 500-degrees-F, electrically heated cabinet oven, currently used for plastic and metal part heat-treating operations at a customer’s facility. Workspace dimensions of the oven are 22 by 21 by 85 in. The Nichrome® wire tubular elements deliver 18 kW to heat the oven chamber, while a 750-CFM, 0.75-HP recirculating blower provides a vertical downward airflow to the workload.

The cabinet oven features 4-in. insulated walls, aluminized steel exterior and interior, three integral metal shelves, and all safety equipment required by NFPA Standard 86 for handling flammable solvents, including a powered forced exhauster, airflow safety switch, and purge timer.

Other controls include a fused disconnect switch, digital temperature controller, and manual reset excess temperature controller.