Practical Welding Today® was created to fill a void in the industry for hands-on information, real-world applications, and down-to-earth advice for welders. No other welding magazine fills the need for this kind of practical information. Subscriptions are free to qualified welding professionals in North America.


More Info Subscribe Free

Selected articles from the January/February 2005 issue available online:

Metallurgy Matters: Thermal cycles, the HAZ, and the strength of martensite

January 18, 2016

By:

Last time we looked at how welding heat influences the heat-affected zone (HAZ) of metals strengthened by three typical hardening processes: solid-solution hardening, cold working, and precipitation hardening. That leaves one critical strengthening process to consider: transformation (martensite)...

Continue Reading

Aluminum Workshop: Passing tensile tests for 6061-T6

December 26, 2014

By:

Q: I am having problems passing the tensile tests for my procedure qualification of aluminum alloy 6061-T6 on 6-inch-diameter pipe, Schedule 120. I am using ER4043 filler metal for a gas tungsten arc welding (GTAW)-gas metal arc welding (GMAW) combination process on the first joint and ER5363 on...

Continue Reading

Arc Welding 101: Wire-feed welding, stick welding with the same machine

November 17, 2014

By:

Q: I would like to know if a wire-feed welding machine can double as a modest-amperage DC shielded metal arc welding (SMAW) machine if I attach an electrode holder to the output. I have been told that aluminum welding works well and is convenient using SMAW and DC. I have the aluminum roller kit...

Continue Reading

Simplifying shielding gas selection

January 11, 2005

By: ,

Have you ever asked yourself any of the following questions: Why is welding affected by the shielding gases used? Why are so many blends available for carbon steel? Why can I use some gases for some materials and not others? Answering these questions will help you take the mystery...

Continue Reading

Optimize your plasma performance

January 11, 2005

By: ,

Plasma arc welding (PAW) uses plasma, a gas that has been heated to a high temperature and ionized. The plasma becomes electrically conductive, transferring an electric arc to the workpiece through a small orifice.