STAMPING Journal®

September/October 2003

STAMPING Journal® is the only industrial publication dedicated solely to serving the needs of the metal stamping market. In 1987 the American Metal Stamping Association broadened its horizons and renamed itself and its publication, known then as Metal Stamping. Print subscriptions are free to qualified stamping professionals in North America.


More Info Subscribe Free

Selected articles from the September/October 2003 issue available online:

R&D Update: Predicting springback in air bending, straight flanging

October 9, 2003

By:

Editor's Note: This column was prepared by the staff of the Engineering Research Center for Net Shape Manufacturing (ERC/ NSM), The Ohio State University, Professor Taylan Altan, director.Air bending and straight flanging are the most prevalent types of bending in sheet metal forming. Predicting...

Continue Reading

Investing in lubricants

October 9, 2003

By:

All businesses tied to the metal forming industry are scrambling to find areas in which they can lower costs without sacrificing quality. Adding to this burden are a tight cash flow and a lack of financial resources to invest in process improvement equipment. Therefore, the savings must come from doing more with less.

Continue Reading

Stamping 101

September 25, 2003

By:

To promote real-world stamping training, the Tooling & Manufacturing Association (TMA) wanted to create a resource whereby stampers could receive a consistent, recognized, hands-on education on the industry's most current equipment.

Continue Reading

Choosing the proper steel to minimize abrasive adhesive tool wear

September 25, 2003

By:

The most disruptive type of failure in any tooling application is when the tool cracks. To prevent this type of failure in cold-work applications, it's important to select the correct steel.

Continue Reading

Hydraulic presses make their mark

September 25, 2003

By:

Just like hydraulics technology itself, the market for presses based on it is fluid and dynamic. And for the first time in a while, the tide may be turning in favor of its practitioners.As many manufacturers report prosperity and strong prospects for it in the near future, the hydraulic press...

Continue Reading