The Tube & Pipe Journal®

October/November 2008

TPJ - The Tube & Pipe Journal® became the first magazine dedicated to serving the metal tube and pipe industry in 1990. Today, it remains the only North American publication devoted to this industry and it has become the most trusted source of information for tube and pipe professionals. Subscriptions are free to qualified tube and pipe professionals in North America.


More Info Subscribe Free

Selected articles from the October/November 2008 issue available online:

Serpentine Bender

Serpentine bending in production

November 25, 2008

By:

Bending serpentine profiles—successive 180-degree bends, which typically are used in refrigeration systems—can be a challenge. By their nature, they tend to cause interference among the various bend dies, and they can be difficult to handle. Good planning in selecting a bender, planning the process, and paying close attention to infeed and outfeed options, can help make a serpentine project successful.

Continue Reading

Roll Former

Selecting speed reducers for roll forming lines

November 11, 2008

By:

Setting up a roll forming line requires careful consideration of the speed reducers to be installed at each forming station. After determining the horsepower for each station, it is necessary to determine the appropriate durability, thermal horsepower rating, and strength for each speed reducer.

Continue Reading

TIG Titanium Tubing

TIG for titanium tubing

October 28, 2008

By:

Although titanium has a reputation for being difficult to weld, it doesn't have to be problematic. Paying close attention to filler metal selection, cleanness, and use of the shielding gas are three steps to successful GTAW on titanium tube and pipe.

Continue Reading

Selecting speed reducers for roll forming lines

October 14, 2008

By:

Setting up a roll forming line requires careful consideration of the speed reducers to be installed at each forming station. After determining the horsepower for each station, it is necessary to determine the appropriate durability, thermal horsepower rating, and strength for each speed reducer.

Continue Reading

Image of forklift

Steady as she goes

October 14, 2008

According to the Bureau of Labor Statistics, in the U.S. nearly 100 workers are killed and another 20,000 are seriously injured annually in forklift-related incidents. Knowing how they occur and studying the events that lead up to them can go a long way in preventing typical accidents.

Continue Reading