AddisonMckee has designed an EB28HS4 electrically powered and hydraulically operated, CNC tube bending machine for a manufacturer of flow control products. The high-speed machine accepts tubing up to 1.10 in. dia. bending up to six... Read more...
AddisonMckee has introduced Hydra Green technology in its new HG70 series of tube end formers. The hydraulic equipment features a pump that is in operation only when there is a demand for pressure and flow. This helps to cut noise and energy... Read more...
AddisonMckee has developed AddiCheck, a noncontact tube measuring and inspection system. The software is suitable for midmarket tube-manipulation companies. The system includes a portable workbench, an optical probe attached to a recently... Read more...