Product
June 13, 2013
Biodegradable liquid cleans metal before finishing
Safe Scrub® ST liquid cleaner from Birchwood provides heavy-duty cleaning power for removing oil and surface soils on metals before finishing. This biodegradable liquid emulsifies oil from iron and steel parts in heavy-duty soak tank... Read more...
-
Product
February 18, 2013
Brush-on blackener serves as quick fix for scratched black oxided parts
PRESTO BLACK® BST4 brush-on liquid from Birchwood® Technologies is an instant-acting cold blackener for all iron and nonstainless steels. When applied to any clean ferrous metal surface, the product blackens within 30 seconds and forms a... Read more...
-
Product
September 13, 2012
Rust blocker has low VOC content
Dri Touch® Amber rust blocker from Birchwood Casey has a low VOC content, high flash point, and almost no odor.
Rated for 100 to 150 hours salt spray and more than 600 hours humidity protection, the rust blocker meets water displacement... Read more...
-
Product
May 10, 2012
Low-VOC rust preventives available in solvent-based, aqueous formulations
Birchwood Casey now offers seven different rust preventive products that are compliant with current VOC regulations recently enacted in several states. The corrosion inhibitors and sealants prevent rust and corrosion on all metal surfaces.... Read more...
-
Product
January 12, 2012
Coatings for iron, steel protect from corrosion
Three corrosion-protection coatings for iron and steel components are available from Birchwood Casey.
The patented TRU TEMP® process, operating at 200 degrees F, produces a high-quality black finish. An in-house line uses no... Read more...
-
Product
August 1, 2011
Aluminum oxide conversion coating introduced
Birchwood Casey has introduced the MICROLOK® AO, a nontoxic aluminum oxide conversion coating that is 0.000060 in. thick, silver-black in color, and tightly adherent to the metal surface.
The patented coating imparts corrosion resistance... Read more...
-
Product
September 21, 2010
30-min. process develops 0.000060-in. black coating
Birchwood Casey offers the scratch-resistant LUMICLAD® finish. The 30-min. process develops a coating thickness of 0.000060 in. with a smooth, clean surface that is electrically conductive and adherent to the aluminum substrate.