April 24, 2013
Large-volume multiaxis laser system guarantees volumetric accuracy
Prima Power Laserdyne has introduced the Laserdyne 795 XLZ. The system has a 72-in. extended Z axis, 80-in. X axis, 40-in.Y axis, and the latest BeamDirector3 (BD3) rotary-tilt laser beam positioning head. The laser is designed to drill,... Read more...

Product

June 28, 2012
Large-format laser system features small footprint
Prima Power Laserdyne offers the model 430 precision laser system. It combines high precision and large-format workholding capabilities for industrial laser welding and cutting. The company will show the system at IMTS 2012 with a... Read more...