June 20, 2011
Metal clinching process helps make quick, clean joints in most ductile materials
The MultiLoc® metal clinching process helps make quick, clean joints in most ductile materials. Powered by a Multicyl® air/oil intensifier, the fast-advance stroke is followed by a smooth hydraulic action.
There are several machine... Read more...
-
Product
October 14, 2008
Linear rail punching systems suitable for applications involving various parts, multiple setups
Multicyl's MultiPunch linear rail (MLR) system is suitable for punching applications that involve a variety of parts and multiple setups. A single machine can punch different part lengths, hole sizes, hole positions, end stop positions, and part... Read more...
-
Article
May 15, 2003
Producing holes in tubing