Article

April 10, 2007
Tooling coating extends die life, reduces die rework
Die sections with a narrow slot, such as the one shown on the right, can be coated with Phygen's low-temperature PVD process without fear of warping the tool. According to Ron Saling, tooling supervisor, Glacier Vandervell Bearings, attempts to... Read more...

Article

December 7, 2004
High-performance coating helps stamper fight downtime
As one of Omni's presses forms the heavy-duty door hinges, a transfer mechanism advances the workpiece to the next station in the die. Because Phyge's FortiPhy™ UltraEndurance™ coating on the four forming inserts inhibits... Read more...