Roll-Kraft Showroom

Visit Roll-Kraft  

 

   Found 2 results for "Roll-Kraft"...

      Just show me: Everything | Articles | News | Products

Product

May 12, 2009
Portable hemming unit forms 180-degree hems
Roll-Kraft has released a portable hemming unit. The machine forms 180-degree hems on the edges of a flat strip of metal. Hems are found primarily on lighter-gauge material to strengthen the profile or improve safety in handling. Typically, the... Read more...

Product

September 11, 2007
Quick-change cutoff system introduced