Harvey Titanium Ltd., a division of Rolled Alloys, now offers CP-1 grade 4 and CP-3 grade 2 sheet titanium. Designed to offer high corrosion resistance and weldability, the titanium grades are available in thicknesses from 0.016 in. to 0.063 in.... Read more...