Sandvik has introduced Sandvik Santronicâ„¢, a coated stainless steel strip designed for electronic component manufacturers. It can serve as an alternative material for postprocessed electroplated parts in stainless steel or copper-based alloys.... Read more...
Sandvik says its new welding strip, Sandvik 24.29.5.LCu, reduces production time by half in overlay welding applications. The material allows users to attain the required grade for 904L overlay in a single weld using a standard flux, the company... Read more...