Tishken Products Company, Founded in 1912, is a leading supplier of high quality roll forming machinery and tooling to the Automotive, Appliance, Building Products, Metal Service Center and Metal Processing Industries.
Roll forming is a continuous bending operation in which a long strip of metal (typically coiled steel) is passed through consecutive sets of rolls, or stands, each performing only an incremental part of the bend, until the desired cross-section profile is obtained. Roll forming is ideal for producing parts with long lengths or in large quantities.