Article
June 30, 2009
Welding aluminum
Selecting an appropriate filler alloy for welding aluminum differs from selecting a filler alloy for welding steels. In the case of steel, selection is primarily a matter of matching the tensile strength of the filler metal to that of the base alloy. For aluminum, many variables come into... Read more...