A new way to weld sheet metal: Remote laser welding replaces spot welding in microwave oven fabrication

Nu-Way Industries Inc., Des Plaines, Ill., learned that remote laser welding demonstrates impressive advantages over traditional resistance and arc welding for its applications.

Publish date: March 7, 2006