June 13, 2006
Measuring the plastic strain ratio of sheet metals Drawing metal successfully relies, in part, on understanding precisely how the metal reacts to tensile forces. When subjected to tensile forces, a flat section of sheet material becomes thinner because of dimensional changes in its width and thickness. The ratio of the changes in width... Read more...