Fatigue Failures Figure 1 Fatigue is the progressive formation and propagation of cracks in a metal subjected to repeated or alternating stresses (from cyclic loads or forces) not exceeding the material's static yield strength limit. The final failure occurs when the remaining section—the part... Read more...