Content tagged with "exhaust"
Results: 2
Article
June 8, 2004
Spraying it right
For coil-fed applications, spray cabinets can be mounted to the feeder to accommodate passline changes. Most stampers understand the need for lubricants, but many apply as little as possible so they don't have to deal with the mess. Others take an opposite approach and flood the tool... Read more...
Article
September 17, 2001
Welding exhaust system components
In the field of automobile exhaust systems, such components as manifolds, pipes, catalytic converters, and mufflers are joined either by the car manufacturer or by a subcontractor to form a subassembly ready for attachment. Today, large numbers of these components are welded with a laser.... Read more...