Easing the grind of cost reduction Automotive parts supplier SPX CONTECH had struggled with quick-attach abrasive fiber disks for its flash removal and deburring of its die-cast aluminum parts. The company found a replacement disk that lasts three times longer than the problem disks. The squeeze on companies in automotive... Read more...