Got burrs?: Making choices for deburring, graining sheet, plateUsing a machine to remove burrs from and put a surface finish on sheet metal and plate, also known as deburring and graining, is more complicated than it seems. The factors that go into selecting and setting up a deburring and graining machine are almost as numerous as the factors that cause burrs in the first place. Some of the important factors you have to consider are machine type (wet or dry), setup (the arrangement of sanding belts and deburring brushes), sanding drum hardness and diameter, brush type, and feed rate.
|
|
Avoiding a snag: Automated deburring ensures nylon-stocking-friendly finishA company specializing in perforated sheet overcomes deburring issues with an automated system using nonwoven fiber brushes.
|