The evolution of precision bending
Photo courtesy of Wila USA, Hanover, Md.
Precision bending has come a long way in recent decades. What used to be considered "precision" in the 1970s wouldn't pass muster today. Then a fabricator might have considered ±1 degree a precision bend; today a precision bend is within a half... Read more...