Comparing single-cut and dimple-free tube mill cutoffs
This article covers the application of single-cut and dimple-free cutoff shear technologies as they are applied to contemporary high-speed tube mills. A single-cut die set is a unit composed of an upper shoe and a lower shoe in which a single severing blade and tube supporting jaws are... Read more...