Article

April 1, 2009
Bending rolled steel sections Bending tube or pipe successfully is a matter of managing a handful of processes and variables. For example, the bending process causes thickening where the metal is under compression and thinning where it is under tension. Too much thickening can result in wrinkles; too much thinning results... Read more...