Maximizing your scrap's value: Diligence in preparation and tracking pays off

The more uniform and contaminant-free that scrap is when fabricators provide it to recyclers, the more fabricators can benefit. This article addresses the two principles for selling scrap to recyclers: know what you're selling vs. what you're getting paid for, and incorporate sorting & cleaning into your production stream.

Publish date: November 29, 2001