Content tagged with "wrinkling"
Results: 4
Article
September 13, 2005
Introduction to advanced high-strength steels
Part I of this two-part series presented an overview of advanced high-strength steels (AHSS). This article addresses issues encountered when processing these grades. Using AHSS in appropriate applications offers opportunities for reduced product weight, enhanced crash performance,... Read more...
Article
September 13, 2005
Introduction to advanced high-strength steels - Part II
Part I of this two-part series presented an overview of advanced high-strength steels (AHSS). This article addresses issues encountered when processing these grades.
Using AHSS in appropriate applications offers opportunities for reduced product weight, enhanced crash performance,... Read more...
Article
August 14, 2003
Toolmaker tricks
This article focuses on a few tricks of the tooling trade that have been used for years. It is very important for toolmakers, troubleshooters, and technicians to make rational data based decisions regarding permanent corrective action. These tricks are intended solely for data gathering purposes... Read more...
Article
January 15, 2001
How to draw round cups deeper
Figure 1 : In deep drawing, sheet metal is forced into a die by a punch to form a part. The draw ratio decreases throughout the process. In general, deep drawing (see Figure 1 ) is a process in which a blank is forced into or through a die by a punch to form a hollow component that... Read more...