Xrize desktop AM platform from Rize offers full-color 3D printing

Rize Inc. offers Xrize, which it says is the world’s first full-color desktop additive manufacturing platform. The company reports that its patented Augmented Deposition technology combines material extrusion and material jetting to deliver industrial-strength parts with minimal postprocessing, complete authentication, and trust by printing text, images, and QR codes.