1960 Seravesi | PCF Series | 4,000 | | | | | 400 | 110 | 70 | 70 | | | | |
1960 Seravesi | PCM Series | 4,000 | | | | | 400 | 78 | 70 | 70 | | | | |
1960 Seravesi | PCF-C Series | 1,000 | | | | | 60 | 51 | | | | | | |
|
AP&T North America, Inc. | LPS-Deep Draw Press | 1,000 | To spec. | | | | To spec. | To spec. | To spec. | To spec. | | | | |
AP&T North America, Inc. | ODEN-FT-8000-28/20 Press Hardening Line | 881 | To spec. | | | | 86.6 | 39.4 | | | | | | |
AP&T North America, Inc. | MSP-Multi Slide Press | 350/station | To spec. | | | | To spec. | To spec. | To spec. | To spec. | | | | |
AP&T North America, Inc. | ODEN-WP | 354 | To spec. | | | | 55.1 | 49.2 | To spec. | To spec. | | | | |
AP&T North America, Inc. | LMB-Blanking Press | 2,000 | To spec. | | | | 31.5 | 19.7 | To spec. | To spec. | | | | |
AP&T North America, Inc. | ODEN-F | 1,406 | To spec. | | | | 78.7 | 63.0 | To spec. | To spec. | | | | |
AP&T North America, Inc. | ODEN-FT-12000-XX/XX Press Hardening Line | 1,223 | To spec. | | | | To spec. | To spec. | To spec. | To spec. | | | | |
|
Amino North America | DRM-300 (Center reversing DSP) | 300 | 196.9 x 110.2 | | | | 98.4 | 70.9 | 31.9 | 165.4 | | | | |
Amino North America | DRM-200 (Center reversing DSP) | 200 | 177.2 x 98.4 | | | | 98.4 | 70.9 | 30.7 | 129.9 | | | | |
Amino North America | DRM-100 (Center reversing DSP) | 100 | 181.1 x 98.4 | | | | 118.1 | 82.7 | 28.3 | 141.7 | | | | |
Amino North America | DSP-600 (Die Spotting Press) | 600 | 196.9 x 102.4 | | | | 94.5 | 66.9 | 23.6 | 141.7 | | | | |
Amino North America | DSP-300 (Die Spotting Press) | 300 | 181.1 x 98.4 | | | | 106.3 | 78.7 | 28.3 | 141.7 | | | | |
Amino North America | DSP-200 (Die Spotting Press) | 200 | 157.5 x 86.6 | | | | 70.9 | 27.6 | 26.0 | 212.6 | | | | |
Amino North America | SDP-2000 (Tryout press) | 2,000 | 196.9 x 102.4 | | | | 126.0 | 106.3 | 21.3 | 590.6 | | | | |
Amino North America | SDP-1200 (Tryout press) | 1,200 | 137.8 x 86.6 | | | | 70.9 | 55.1 | 26.0 | 826.8 | | | | |
Amino North America | SDP-500 (Tryout press) | 500 | 118.1 x 78.7 | | | | 86.6 | 66.9 | 21.3 | 354.3 | | | | |
Amino North America | SDP-200 (Tryout press) | 200 | 59.1 x 47.2 | | | | 31.5 | 19.7 | 23.6 | 472.4 | | | | |
|
Baileigh Industrial Inc. | CFP-45HD | 45 | 27.56 x 23.625 x 1.75 | | | | 20 | 16.5 | 16.8 | 108 | | | | |
Baileigh Industrial Inc. | CFP-70HD | 70 | 27.56 x 23.625 x 1.75 | | | | 20.6 | 16.5 | 16.8 | 108 | | | | |
Baileigh Industrial Inc. | CFP-112HD | 112 | 31.5 x 20.86 x 3 | | | | 21 | 18 | 16.8 | 108 | | | | |
|
Beckwood Press Co. | Gib-guided | 10,000 | To spec. | | | | To spec. | To spec. | To spec. | To spec. | | | | |
Beckwood Press Co. | Four-post | 2,500 | To spec. | | | | To spec. | To spec. | To spec. | To spec. | | | | |
Beckwood Press Co. | Two-post | 200 | To spec. | | | | To spec. | To spec. | To spec. | To spec. | | | | |
Beckwood Press Co. | C-Frame | 500 | To spec. | | | | To spec. | To spec. | To spec. | To spec. | | | | |
Beckwood Press Co. | Benchtop | 55 | | | | | | 7.9 | 113 | 940 | | | | |
Beckwood Press Co. | Stretch Former | 1,000 | To spec. | | | | To spec. | To spec. | To spec. | To spec. | | | | |
Beckwood Press Co. | Joggle Former | 1,000 | To spec. | | | | To spec. | To spec. | To spec. | To spec. | | | | |
Beckwood Press Co. | Ring Expander | 1,000 | To spec. | | | | To spec. | To spec. | To spec. | To spec. | | | | |
Beckwood Press Co. | Sheet Hydroform | To spec. | To spec. | | | | | | | | | | | |
|
Danly and Verson by Enprotech | Hot & Cold Drawing & Forming | 12,000 | 250 x 200 | | | | 150 | 125 | 60 | 1,500 | | | | |
Danly and Verson by Enprotech | Die Tryout | 3,000 | 250 x 125 | | | | 125 | 100 | 60 | 1,500 | | | | |
Danly and Verson by Enprotech | Hemming Press | 300 | 125 x 125 | | | | 100 | 75 | 30 | 500 | | | | |
Danly and Verson by Enprotech | Hot & Cold Forging | 15,000 | 150 x 150 | | | | 200 | 175 | 180 | 1,500 | | | | |
Danly and Verson by Enprotech | Hot & Cold Extrusion | 5,000 | 125 x 125 | | | | 200 | 175 | 180 | 1,500 | | | | |
Danly and Verson by Enprotech | Chassis Frame | 7,500 | 500 x 75 | | | | 100 | 75 | 45 | 1,000 | | | | |
Danly and Verson by Enprotech | Transfer (multistation) | 5,000 | 500 x 125 | | | | 100 | 75 | 60 | 1,000 | | | | |
Danly and Verson by Enprotech | SMC/FRP/GMT Compression | 3,000 | 250 x 150 | | | | 150 | 125 | 30 | 1,000 | | | | |
Danly and Verson by Enprotech | Multiplaten Compression | 15,000 | 150 x 100 | | | | 125 | 125 | 15 | 100 | | | | |
Danly and Verson by Enprotech | Die Spotting | 500 | 200 x 100 | | | | 100 | 75 | 30 | 250 | | | | |
|
Eagle Press & Equipment Co. Ltd. | SH1 Straight-Side Single Point | 50-500 | To 60 x 60 | | | | To spec. | To spec. | To spec. | To spec. | | | | |
Eagle Press & Equipment Co. Ltd. | SH2 Straight-Side Two Point | 100-1,200 | To 180 x 60 | | | | To spec. | To spec. | To spec. | To spec. | | | | |
Eagle Press & Equipment Co. Ltd. | SH4 Straight-Side Four Point | 800-4,000 | To 320 x 120 | | | | To spec. | To spec. | To spec. | To spec. | | | | |
Eagle Press & Equipment Co. Ltd. | PH1 4 Post Single Point | 50-200 | To 60 x 60 | | | | To spec. | To spec. | To spec. | To spec. | | | | |
Eagle Press & Equipment Co. Ltd. | PH2 4 Post Two Point | 50-600 | To 180 x 96 | | | | To spec. | To spec. | To spec. | To spec. | | | | |
|
Erie Press Systems | Hydraulic Presses | 10,000 | To spec. | | | | To spec. | To spec. | To spec. | To spec. | | | | |
|
Fagor Arrasate USA Inc. | Monoblock Deep Draw Press | 1,000 | Max. 118 x 79 | | | | To spec. | To spec. | To spec. | To spec. | | | | |
Fagor Arrasate USA Inc. | Special-Purpose Presses | 800 | To spec. | | | | To spec. | To spec. | To spec. | To spec. | | | | |
Fagor Arrasate USA Inc. | Tryout Presses | 3,000 | To spec. | | | | To spec. | To spec. | To spec. | To spec. | | | | |
Fagor Arrasate USA Inc. | Production Presses | 3,000 | To spec. | | | | To spec. | To spec. | To spec. | To spec. | | | | |
Fagor Arrasate USA Inc. | Press Hardening | 2,500 | To spec. | | | | To spec. | To spec. | To spec. | To spec. | | | | |
Fagor Arrasate USA Inc. | Composite Standard Press | 3,600 | To spec. | | | | To spec. | To spec. | To spec. | To spec. | | | | |
Fagor Arrasate USA Inc. | Composite HLC Press | 3,600 | Max. 141 x 94 | | | | 126 | 95 | 188 | 1,880 | | | | |
|
Freeman Schwabe Machinery | 4-Post | 5,000 | To spec. | | | | To spec. | To spec. | To spec. | To spec. | | | | |
Freeman Schwabe Machinery | 4-Post High Stroke (4PHS) | 5,000 | To spec. | | | | To spec. | To spec. | To spec. | To spec. | | | | |
Freeman Schwabe Machinery | SR Straight Ram | 5,000 | To spec. | | | | To spec. | To spec. | To spec. | To spec. | | | | |
Freeman Schwabe Machinery | CM Compression Molding | 5,000 | To spec. | | | | To spec. | To spec. | To spec. | To spec. | | | | |
Freeman Schwabe Machinery | High-Speed Die Cutting Press | 110 | 20-31 x 20-39 | | | | | | | | | | | |
Freeman Schwabe Machinery | Traveling Head Automatic Press A7A | 125 | 64 x 120, 20 x 40 | | | | | | | | | | | |
Freeman Schwabe Machinery | Full Head Press | 300 | 19-78 x 35-98 | | | | | | | | | | | |
Freeman Schwabe Machinery | Schwabe Model D Clicker Press | 25 | 18 x 36, 20 x 40 | | | | | 3 | | | | | | |
Freeman Schwabe Machinery | Receding Head / Beam Press | 220 | 23-59 x 35-98 | | | | | | | | | | | |
|
Gigant Italia S.r.l. | GTP C-Frame | 40-315 | 51 x 24 | | | | 40 | 32 | 165 | 1,181 | | | | |
Gigant Italia S.r.l. | GTP C-Frame | 40-350 | To spec. | | | | To spec. | To spec. | To spec. | To spec. | | | | |
Gigant Italia S.r.l. | G2 Straight-Frame | 100-2,000 | To 200 x 100 | | | | 80 | 60 | 130 | 1,181 | | | | |
Gigant Italia S.r.l. | G2 Straight-Frame | 3,000 | To spec. | | | | To spec. | To spec. | To spec. | To spec. | | | | |
Gigant Italia S.r.l. | G2 Blanking | 70-600 | To spec. | | | | To spec. | To spec. | To spec. | 1,181 | | | | |
Gigant Italia S.r.l. | G2 Tryout | 2,000 | To spec. | | | | To spec. | To spec. | 130 | 1,181 | | | | |
Gigant Italia S.r.l. | Hot Forging | 1,000 | To spec. | | | | To spec. | To spec. | To spec. | To spec. | | | | |
Gigant Italia S.r.l. | G2 Transfer | 200-1,200 | To spec. | | | | To spec. | To spec. | 130 | 1,181 | | | | |
Gigant Italia S.r.l. | G2 Tandem Line | 200-2,500 | To spec. | | | | To spec. | To spec. | To spec. | To spec. | | | | |
|
Greenerd Press & Machine Co. Inc. | GG, FT, Gib-guided | 10,000 | To spec. | | | | To spec. | To spec. | To spec. | To spec. | | | | |
Greenerd Press & Machine Co. Inc. | HPB, Bench Press | 75 | To spec. | | | | To spec. | To spec. | To spec. | To spec. | | | | |
Greenerd Press & Machine Co. Inc. | 4D, Four-post | 10,000 | To spec. | | | | To spec. | To spec. | To spec. | To spec. | | | | |
Greenerd Press & Machine Co. Inc. | HCA, Gap-frame | 10,000 | To spec. | | | | To spec. | To spec. | To spec. | To spec. | | | | |
Greenerd Press & Machine Co. Inc. | CAP, Air-over-oil | 250 | To spec. | | | | To spec. | To spec. | To spec. | To spec. | | | | |
|
Interlaken Technology Company, LLC | SP75 | 37.5 | 18 x 19 | | | | 16 | 12 | 30 | 30 | | | | |
Interlaken Technology Company, LLC | SP150 | 75 | 28.6 x 31 | | | | 24 | 14.9 | 660 | 660 | | | | |
Interlaken Technology Company, LLC | SP225 | 112 | 28.6 x 38 | | | | 28 | 14.9 | 472 | 472 | | | | |
Interlaken Technology Company, LLC | SP400 | 183.5 | 17.2 x 33.5 | | | | 22.25 | 8 | 60 | 60 | | | | |
Interlaken Technology Company, LLC | SP600 | 300 | 34.3 x 56 | | | | 37 | 24 | 180 | 180 | | | | |
|
KAAST Machine Tools, Inc. | HPC C-Frame | 440 | 40 x 24 | | | | 30 | 20 | 600 | 600 | | | | |
KAAST Machine Tools, Inc. | HPA Workshop | 220 | 60 x 16 | | | | 60 | 12 | 30 | 20 | | | | |
KAAST Machine Tools, Inc. | HPF H-Frame | 1,000 | 60 x 40 | | | | 48 | 24 | 300 | 120 | | | | |
KAAST Machine Tools, Inc. | HPQ 4-Post | 220 | 50 x 40 | | | | 24 | 20 | 60 | 60 | | | | |
KAAST Machine Tools, Inc. | HPP C-Frame | 165 | 20 x 12 | | | | 15 | 15 | 180 | 180 | | | | |
|
KNUTH Machine Tools USA Inc. | KNWP 60 HM Workshop Press | 66 | 30 x 10 | | | | | 15 | 4.8 | 25.2 | | | | |
KNUTH Machine Tools USA Inc. | KNWP 100 HM Workshop Press | 110 | 43 x 12 | | | | | 15 | 6 | 21.6 | | | | |
KNUTH Machine Tools USA Inc. | KNWP 160 HM Workshop Press | 176 | 43 x 15 | | | | | 16 | 5.4 | 22.2 | | | | |
KNUTH Machine Tools USA Inc. | KP 70 A H-Frame Press | 77 | 31 x20 | | | | | 19.7 | 12 | 52 | | | | |
KNUTH Machine Tools USA Inc. | KP 100 A H-Frame Press | 110 | 35 x 24 | | | | | 19.7 | 9.6 | 52 | | | | |
KNUTH Machine Tools USA Inc. | KP 150 A H-Frame Press | 165 | 47 x 28 | | | | | 19.7 | 7.2 | 52 | | | | |
KNUTH Machine Tools USA Inc. | HPK 40 A C-Frame Press | 44 | 27.5 x 19.5 | | | | | 19.7 | 21 | 60 | | | | |
KNUTH Machine Tools USA Inc. | HPK 70 A C-Frame Press | 77 | 27.5 x 19.5 | | | | | 19.7 | 12 | 60 | | | | |
KNUTH Machine Tools USA Inc. | HPK 100 A C-Frame Press | 110 | 31.5 x 23.5 | | | | | 19.7 | 9.6 | 60 | | | | |
KNUTH Machine Tools USA Inc. | HPK 150 A C-Frame Press | 165 | 31.5 x 23.5 | | | | | 19.7 | 7.2 | 60 | | | | |
|
Lauffer Pressen / EuroPress Metalforming | SRZ, Servo-Hydraulic Press | 1,100 | To spec. | | | | To spec. | To spec. | To spec. | To spec. | | | | |
Lauffer Pressen / EuroPress Metalforming | RZU, Deep Draw | 2,200 | To spec. | | | | To spec. | To spec. | To spec. | To spec. | | | | |
Lauffer Pressen / EuroPress Metalforming | RZX, Deep Draw (Triple) | 2,200 | To spec. | | | | To spec. | To spec. | To spec. | To spec. | | | | |
Lauffer Pressen / EuroPress Metalforming | RPS, General-purpose / heavy duty | 440 | To 48 x 40 | | | | 25 | 18 | To spec. | To spec. | | | | |
Lauffer Pressen / EuroPress Metalforming | RPT, General-purpose | 440 | To 48 x 40 | | | | 25 | 18 | To spec. | To spec. | | | | |
Lauffer Pressen / EuroPress Metalforming | Tryout & Custom Presses | 4,000 | To spec. | | | | To spec. | To spec. | To spec. | To spec. | | | | |
Lauffer Pressen / EuroPress Metalforming | RKP, Composite | 4,000 | To spec. | | | | To spec. | To spec. | To spec. | To spec. | | | | |
Lauffer Pressen / EuroPress Metalforming | EPT, C-Frame | 300 | To 48 x 40 | | | | 25 | 18 | To spec. | To spec. | | | | |
Lauffer Pressen / EuroPress Metalforming | RPM-SE, Powder Metal Compacting | 1,800 | To spec. | | | | To spec. | To spec. | 125 | 800 | | | | |
Lauffer Pressen / EuroPress Metalforming | RA, Powder Metal Calibrating | 1,500 | To spec. | | | | To spec. | To spec. | 125 | 800 | | | | |
|
Macrodyne Technologies Inc. | Hydraulic Presses | 20,000 | To spec. | | | | To spec. | To spec. | To spec. | To spec. | | | | |
Macrodyne Technologies Inc. | Metalforming Presses | 1,200 | To spec. | | | | To spec. | To spec. | To spec. | To spec. | | | | |
Macrodyne Technologies Inc. | Compression Molding Presses | 3,000 | To spec. | | | | To spec. | To spec. | To spec. | To spec. | | | | |
Macrodyne Technologies Inc. | Forging Presses | 20,000 | To spec. | | | | To spec. | To spec. | To spec. | To spec. | | | | |
Macrodyne Technologies Inc. | Hot Stamping Presses | 3,000 | To spec. | | | | To spec. | To spec. | To spec. | To spec. | | | | |
Macrodyne Technologies Inc. | Hydroforming Presses | 3,000 | To spec. | | | | To spec. | To spec. | To spec. | To spec. | | | | |
Macrodyne Technologies Inc. | Deep Draw Presses | 2,000 | To spec. | | | | To spec. | To spec. | To spec. | To spec. | | | | |
Macrodyne Technologies Inc. | Cold Forming Presses | 2,000 | To spec. | | | | To spec. | To spec. | To spec. | To spec. | | | | |
Macrodyne Technologies Inc. | Electrically Heated Presses | 1,500 | To spec. | | | | To spec. | To spec. | To spec. | To spec. | | | | |
Macrodyne Technologies Inc. | Supeplastic Forming Presses | 600 | To spec. | | | | To spec. | To spec. | To spec. | To spec. | | | | |
|
Marando Industries, Inc. | Hydroform Press | 5,500 | 85 x 124 | | | | | 950 | | 800 | | | | |
Marando Industries, Inc. | RoboClamp-Hydroform | 20,000 | 32 x 177 | | | | | 1,200 | | 1,200 | | | | |
Marando Industries, Inc. | Hot Stamping Press | 1,800 | 70 x 100 | | | | | 1,200 | | 950 | | | | |
Marando Industries, Inc. | Hydraulic Press | 5,500 | 85 x 124 | | | | | 1,200 | | 950 | | | | |
Marando Industries, Inc. | Pipe Forming Press | 11,000 | 75 x 700 | | | | | | | | | | | |
|
Multipress Inc. | W6A Bench | 3 | To spec. | | | | To spec. | To spec. | To spec. | To spec. | | | | |
Multipress Inc. | M5P Bench | 20 | To spec. | | | | To spec. | To spec. | To spec. | To spec. | | | | |
Multipress Inc. | FMS & FMD Floor | 300 | To spec. | | | | To spec. | To spec. | To spec. | To spec. | | | | |
Multipress Inc. | 4 Post | 1,200 | To spec. | | | | To spec. | To spec. | To spec. | To spec. | | | | |
|
Pacific Press Technologies | Ecoformer | 300 | To spec. | | | | 23 | 18 | To spec. | To spec. | | | | |
Pacific Press Technologies | Ecoformer G | 300 | To spec. | | | | 23 | 18 | To spec. | To spec. | | | | |
Pacific Press Technologies | Pressformer II | 1,000 | To spec. | | | | 60 | 60 | To spec. | To spec. | | | | |
Pacific Press Technologies | Pressformer II Gibbed | 375 | To spec. | | | | 60 | 60 | To spec. | To spec. | | | | |
Pacific Press Technologies | OBL Straight-side | 1,500 | To spec. | | | | 72 | 72 | To spec. | To spec. | | | | |
Pacific Press Technologies | OBM Straight-side | 1,500 | To spec. | | | | 72 | 72 | To spec. | To spec. | | | | |
Pacific Press Technologies | D Column | 3,000 | To spec. | | | | 72 | 72 | To spec. | To spec. | | | | |
Pacific Press Technologies | M Column | 1,500 | To spec. | | | | 72 | 72 | To spec. | To spec. | | | | |
Pacific Press Technologies | Horizontal | 1,250 | To spec. | | | | 48 | 48 | To spec. | To spec. | | | | |
Ravne Presses Ravne na Koroškem, Slovenia |
Ravne Presses | SH1 Straight-Side Presses | 630 | 78 x 78 | | | | 63 | 40 | 120 | 500 | | | | |
Ravne Presses | SH2 Straight-Side Presses | 1,000 | 120 x 78 | | | | 71 | 40 | 95 | 400 | | | | |
Ravne Presses | Tryout Presses | 2,500 | To spec. | | | | To spec. | To spec. | To spec. | To spec. | | | | |
Ravne Presses | Forging Presses | 3,500 | To spec. | | | | To spec. | To spec. | To spec. | To spec. | | | | |
Ravne Presses | Custom Presses | 4,000 | 360 x 100 | | | | To spec. | To spec. | 300 | 1,200 | | | | |
|
SIMPAC America Co., Ltd | PH/PDH Series | 2,755 | 177.1 x 98.4 | | | | 78.7 | 78.7 | 600 | 600 | | | | |
SIMPAC America Co., Ltd | PTS2 series | 2,204 | 177.1 x 98.4 | | | | 98.4 | 78.7 | 600 | 600 | | | | |
|
SWH Precision/Formtechnic | OMERA OPI.M Monolithic Frame | 1,000 | 98 x 63 | | | | 59 | 48 | 6 | 26 | | | | |
SWH Precision/Formtechnic | OMERA OPI.T Composite Frame | 2,000 | 197 x 98 | | | | 59 | 48 | 6 | 26 | | | | |
SWH Precision/Formtechnic | OMERA OPI.C C-Frame Press | 200 | 39 x 32 | | | | 39 | 26 | 6 | 26 | | | | |
|
Sahinler Metal Makina | HKP-Z 30 | 33.7 | 23.6 x 35.4 | | | | | 11.8 | 42.5 | 390 | | | | |
Sahinler Metal Makina | HKP-Z 100 | 112.4 | 27.6 x 43.3 | | | | | 19.7 | 20.1 | 390 | | | | |
Sahinler Metal Makina | HKP-Z 150 | 169 | 29.5 x 47.2 | | | | | 19.7 | 20.1 | 390 | | | | |
Sahinler Metal Makina | HKP-Z 60 | 67.4 | 23.6 x 39.4 | | | | | 13.8 | 23.6 | 390 | | | | |
|
Savage Engineering and Sales Inc. | Deep Draw | 350 | 60 x 48 | | | | 36 | 24 | To spec. | To spec. | | | | |
Savage Engineering and Sales Inc. | Straight Side | 1500 | 72 x 48 | | | | 48 | 36 | To spec. | To spec. | | | | |
Savage Engineering and Sales Inc. | 4 Post | 100 | 32 x 32 | | | | 24 | 18 | To spec. | To spec. | | | | |
Savage Engineering and Sales Inc. | 4 Post | 1,000 | 96 x 72 | | | | 120 | 55 | To spec. | To spec. | | | | |
Savage Engineering and Sales Inc. | Hot Extrusion | 400 | 26 x 24 | | | | 36 | 28 | To spec. | To spec. | | | | |
Savage Engineering and Sales Inc. | Horizontal | 400 | 36 x 90 | | | | 240 | 30 | To spec. | To spec. | | | | |
Savage Engineering and Sales Inc. | Gantry Straightening | 1850 | 36 x 360 | | | | 30 | 24 | To spec. | To spec. | | | | |
Savage Engineering and Sales Inc. | C Frame Guided | 500 | 36 x 30 | | | | 30 | 24 | To spec. | To spec. | | | | |
Savage Engineering and Sales Inc. | Die Repair | 1,000 | 36 x 30 | | | | 30 | 24 | To spec. | To spec. | | | | |
Savage Engineering and Sales Inc. | MetalFormer | 750 | 60 x 48 | | | | 55 | 36 | To spec. | To spec. | | | | |
|
Schuler Inc. | Single Press: SH160 to SH400 | 440 | 52 x 40 to 64 x 112 | | | | 60 | To spec. | To spec. | To spec. | | | | |
Schuler Inc. | Single Press: SH500 to SH800 | 880 | 64 x 52 to 112 x 64 | | | | 60 | To spec. | To spec. | To spec. | | | | |
Schuler Inc. | Single Press: SH1000 to SH1600 | 1,760 | 80 x 52 to 112 x 64 | | | | 80 | To spec. | To spec. | To spec. | | | | |
Schuler Inc. | Tandem Line Presses: SH500 to SH800 | 880 | 72 x 104 to 100 x 164 | | | | 80 | To spec. | To spec. | To spec. | | | | |
Schuler Inc. | Tandem Line Presses: SH1000 to SH2500 | 2,800 | 72 x 124 to 112 x 200 | | | | 108 | To spec. | To spec. | To spec. | | | | |
Schuler Inc. | Transfer Presses | 3,600 | 283 x 122 | | | | 98 | To spec. | To spec. | To spec. | | | | |
Schuler Inc. | Die Spotting & Tryout Presses | 3,000 | 196 x 100 | | | | To spec. | To spec. | To spec. | To spec. | | | | |
Schuler Inc. | Hydroform Press | 2,500 | 125 x 85 | | | | To spec. | To spec. | To spec. | To spec. | | | | |
Schuler Inc. | Hydroform Press | 5,000 | 138 x 99 | | | | To spec. | To spec. | To spec. | To spec. | | | | |
Schuler Inc. | Hydroform Press | 3,500 | 138 x 99 | | | | To spec. | To spec. | To spec. | To spec. | | | | |