ROLEI PEF 500 (Hand Tool)     D 1         .75   2,800 RPM  
ROLEI EF 165 (Hand Tool)     D 1         .75   2,800 RPM  
ROLEI BE 5 (Hand Tool)     D 2     6.5   .50 600 RPM 1,200 RPM  
ROLEI EF 115 (Hand Tool)     D 1     4.5   1.20 2,000 RPM 7,600 RPM  

 HANS WEBER Paola, KS United States   Hot Link

NLC 60 6 W 4 8   30 3 30  
TT1P167 60 4 D 3 7.25   25 3 30 1,800
TTSC 52 8 D 1-2 7.25   15 3 30 1,200
MK 79 4 D 1-4 6   30 3 30 2,200
TN 52 8 W 1-3 6   15 3 30  

 AM MACHINERY SALES INC. Warminster, PA United States

DiscMaster 4TD 39, 60 1 D 2     10   2 39.4 197 1,800
CrossMaster DD 6, 12 1 D 2     16   1.2 39.4 394 1,200
BeltMaster K4TD-1350 53 10 D 3 10   20 39.4 197 2,200
CrossMaster 2TD-500 20 1 D 2   10   2 39.5 236 1,200
DiscMaster SF 1/1 39, 60 10 D 2     6   5 20 157.5 1,800
DiscMaster SF 2/2 39, 60 10 D 4     6   5 20 157.5 2,200

 AME ABRASIVE BELT MACHINERY & EQUIPMENT INC. Delta, BC Canada

SG630-WJS+DB 24 10.5 W 3 Disc: 6, Brush: 8          
SG-1030-WJS+2D+B Vacuum 40 5 W 4 6.63 O   78 400  
SG1600-2WJS+B 62 19.5 W 3              
SD-H Vacuum Table 1 1 D 2   6   1      
SB1000 39.3 5.9 D 2               2 side in one pass

 BLAST & WASH SYSTEMS Wayland, New York United States

4836 V Roller Blast 48 36 D 4 blast wheels           25 24 96 5,000

 FLADDER Atlanta, GA United States

AUT 39, 47     6       13.8     12 394  
300 Gyro 51.5, 63     6       13.8     12 394  
400 Gyro 51.5, 63     6       13.8     12 394  
300 LS 5.75     2-8       5.75     20 1,950  

 GAUER METAL PRODUCTS INC. Kenilworth, NJ United States

5H-Series (Rolled Edge) .625, 52 1 D 2             12 1,200 No Dust
6H-10 (Round Edge) .625, 10 1 D 6             12 1,500 No Dust
9H-10 (Rugged Duty) .50, 10 1 D 6             12 1,500 No Dust
9H-CTL Safety Edger .50, 10 1 D 6           46 12 3,000 No Dust
8H-CTL Safety Edger .75, 10 1 D 4-6           53 12 2,400 No Dust
10H-Bar Deburring Master 1, 8 36 D 4           53 12 1,500 No Dust
10H-CTL Safety Edger 1, 8 1 D 4           78 12 2,400 No Dust

 HECK INDUSTRIES INC. Hartland, MI United States

8000     D             1 0 .625  
12-C Bevel-Mill                       .625  
VA-400 .50 .50 D 1                  
Weld Shaver .50   D 1       4   3      
Turbo-Burr No max. No min. D 1       .25         6

 LISSMAC CORPORATION Waterford, NY United States

SBM Oxide Removal 39/59 6 D 2           0 157  
SBM Edge Rounding 39/59 6 D 2-4           0 157 3,200-8,500
Steelmaster Surface Finishing 37/64 11 D 5       47 393 3,200-8,500
Steelmaster Surface Finishing 37/64 11 W 4       47 393  

 METALFINISH Plainville, CT United States

Ernst Pluto/Titan HD Deslagging 80 3.2 D 3   17   Up to 30 20 200 2,500-3,400
Ernst Atlas Series 60 3.2 D 1-16 8-17   Up to 30 20 400 3,200-8,500
Ernst Neptun Wet Series 60 3.2 W 1-16 8-17   Up to 30 20 400  
NS DM 1100/1600 Deburring/Edge Rounding 64 2 D 1-3   Cross Belt   Up to 40 20 320 1,800-3,200
NS DM 660 Z-PK Extreme Edge Rounding 26 3 D 1-3   Rotor 14   Up to 20 20 400 3,600-8,500
NS FG Series 13 4 D 1-4   6-12   Up to 15 40 800 1,200
NS TR120 Series Edge Grinder 12 8 D 1-8   6-12 O 4.5 40 600 600
NS LR 30 AT Open 2 D 2     10   4 20 240 600
NS - Oxide Removal 44 7 D 2     Cross Belt   7.5 20 200 2,500
Gecam G3 Series TT 12 6 D 1-3 6-10   Up to 5.5 40 400 600
Gecam G6 Series 26 6 D 1-4 6-10   7.5 40 400 Up to 1,800
Gecam G11 Series 44 6 D 1-4 6-10   15 40 400 Up to 3,300
Gecam G13 Series 51 8 D 1-4 8-12   20 40 400 Up to 4,600
Gecam G16 Series 64 8 D 1-4 8-12   Up to 25 40 400 Up to 6,800
Gecam Wet G6/G13 26 / 51 8 W 1-4 6-12   7.5-20 40 400  
Gecam GT13-S Edge Rounding 51 6 D 2-3 Top and Bottom   Drum 8 - Cross Belt   Up to 25 20 320 Up to 3,300
Gecam GT1-B Oxide Removal 51 6 D 2 Top and Bottom     Cross Belt   7.5 20 320 2,500

 SLIPCON USA INC. / APEX MACHINE GROUP Burnsville, MN United States

Perfection BBDD 53 4 D 2 Rollers, 11 Discs   Roller: 11.25, Disc: 9.75 O 3 0 45  
Perfection 2DD-1350 52 4 D 22 Discs     Disc: 9.75 O 3 3 45  
Perfection 2DD-1850 72 4 D 30 Discs     Disc: 9.75 O 3 3 45  
MetalPro EZ3760-M 36 6 D 1     6   10 3 25  
Apex 5275-4TW 52 10 W 1 - 4   Drum: 8 O 15-40 3 25  
Apex 3775-4TD 36 7 D 1 - 4 Drum: 8, Disc: 4, Brush: 8 O 15-30 3 25  
Apex 2575-1TD 24 5 D 1 - 4 Drum: 4, Disc 4, Brush 6 O 10-20 3 25  
Apex 1975-4TW 18 7 W 1 - 4   Drum: 6, Brush: 6   10-25 3 25  

 SUPERMAX TOOLS St. Paul, MN United States

SuperBrush 24 with Vacuum Hold-down 24 3 D 1     Var.   5 0 30 600
SuperBrush 24 24 10 D 1     Var.   5 0 15 600
SuperBrush 36 36 10 D 1     Var   5 0 15 600
SuperBrush 36 Double Head 36 10 D 2     Var.   5 0 30 800
SuperBrush 49 48 10 D 1     Var.   5 0 15 800
WideBelt 25 24 10 D 1     60   10 or 20 15 60 800
WideBelt 37 36 10 D 1     60   15 or 20 15 60 800

 TIMESAVERS INC. Maple Grove, MN United States

Mini-Belt 8 5.5 D 1     3.25   5 15 15 500
1100 Series 8 5 W 1 - 2     3.25   5 10 30  
1200 Series 8, 24, 36 5 - 8.5 D 1 - 2     3.25 - 6   5 - 15 10 45 Var.
1221-11-05 8 1 Sq. D 2   3.25, 14   5 10 30 500
1200 Slag Grinder 36 8 D 2     6   15 - 10 10 25 1,000
2100 Series 36 8 W 1     6   10 - 15 15 45  
2200 Series 36, 51 9, 10 D 1 - 3   6 - 8 O 15 - 30 15 45 Var.
2200 Slag Grinder 36 10.75 D 3   6, 8 O 25, 20 10 30 4,500 (Total)
2200 Rotary Brush 51 4 Sq. D 1     12   10 5 30 5,250
Lynx (19MWT) 18 8 W 1 - 4   6 O 20 10 30  
Lynx (37MWT) 36 8 W 1 - 4   6 O 15 -20 15 45
PUMA (52MWT) 51 10 W 1 - 4   8 O 15 - 30 5 25  
4100 Series Disc 24, 36, 51 3 Sq. W 1 - 3 Drum: 7 Disc: 36/48/60 O 5 - 30 3 30  
4200 Series 36, 51 11 - 13.5 D 1 - 4   7, 11 O 15 - 40 15 65 Var.
4200 Slag Grinder 36, 51 13.5 D 3   7, 11 O 30, 30, 25 10 30 3,000 or 4,400 (Total)