GMAW Power Source Buyers' Guide©

Model
or
Series
Type of
Power
Source
Wire Feed
Options
Wire Feed
Speed
Range
Running Gear Std. Applicable Processes Output Rating (DC) Input Rating
GTAW GMAW SMAW FCAW GMAWP GTAWP Carbon Arc Brazing Spot CACA SAW Other Gouging Amps Voltage Duty Cycle Volts Phase Hz

 Hot Link - ESAB Welding & Cutting Products - GMAW ESAB WELDING & CUTTING PRODUCTS Florence, SC United States  

Caddy Mig C200i
Inverter
Built-in
78-472
                      
180
23
25
230
1
50/60
Migmaster 215 Pro
Tapped Xfmr/Rectifier
Built-in
75-700
                   
250
23
20
208/230
1
60
Migmaster 280 Pro
Tapped Xfmr/Rectifier
Built-In
55-770
                   
300
29
40
208/230
1
60
Warrior 500i
Microbased Inverter, Multiprocess (CV/CC)
External Dedicated
32 - 1,000
                
500
40
60
380/460
3
50/60
Origo Mig 320
Tapped Xfmr/Rectifier
External
31 - 1,000
                    
320
30
30
230/460
3
60
Origo Mig 410
Tapped Xfmr/Rectifier
External
31 - 1,000
                    
400
34
50
230/460
3
60
Mig 4002c, 4002cw
Chopper CV/CC
External
32 - 1,000
       
400
34
60
230/460
3
50/60
Mig 6502c, 6502cw
Chopper CV/CC
External
32 - 1,000
       
650
44
60
230/460
3
50/60
Aristo Mig U5000i
Microbased Inverter, Multiprocess (CV/CC)
External Dedicated
32 - 1,000
       
500
39
60
460
3
60
Aristo Mig U5000iw
Microbased Inverter, Multiprocess (CV/CC)
External Dedicated
32 - 1,000
       
500
39
60
460
3
60

 Hot Link - OTC Daihen Inc. - GMAW OTC DAIHEN INC. Tipp City, OH United States  

HD-500
SCR
External
20 - 780
                        
500
45
50
230/460
3
50/60
DW-300
Inverter
External
20 - 780
                        
300
29
80
460
3
50/60
DA-300P
AC + DC
External
20 - 780
                        
4 - 300
22 - 30
40
460
3
50/60
DL-350
Inverter
External
20 - 780
                          
350
36
60
200
3
50/60
MIG 135
DC CV Spool Gun
Spool Gun
                                
20
230/460/575
1
 

 INTERNATIONAL WELDING EQUIPMENT North Fort Myers, FL United States

HYL MIG130 Multiprocess MIG/TIG/Stick
Inverter
Built-in
30-500
                      
130
25
40@130
110
1
50/60
HYLMIG180Y
Inverter
Built-in
50-600
                          
180
28
60@180
220
1
50/60
HYL MIG200Y
Inverter
Built-in
50-600
                      
200
29
60@200
220
1
50/60
HYL MIG250Y
Inverter
Built-in
50-700
                      
250
29
60@250
29
1
50/60
HYL MIG350H
Inverter CC/CV
External
50-800
                    
350
29
100@350
220
3
50/60
HYLMIG500h
Inverter CC/CV
External
50-800
                    
500
29
100@500
460
3
50/60

 LIBURDI ENGINEERING LTD. Dundas, ON Canada

OrbiMIG II
Inverter
External
800
                          
350
34
60
208/230/400/460/575
3
50/60

 LINCOLN ELECTRIC CO., THE Cleveland, OH United States

POWER MIG® 140C
Rectifier
Built-in
50 - 500
                        
30 - 140
19.5
20@90A, 19.5V
120
1
60
POWER MIG® 180C
Rectifier
Built-in
50 - 500
                        
30 - 180
20
30@130A, 20V
208/230
1
60
POWER MIG® 180 Dual
Rectifier
Internal
50-500 IPM
                        
30-180
34
20@19.5V, 90A on 120V: 30@20V, 130A on 230V
120/208/230
1
60
POWER MIG® 216
Rectifier
Built-in
50 - 700
                      
30 - 250
40
30@216A, 22V
208/230V
1
50/60
POWER MIG® 256
Rectifier
Built-in
50 - 700
                      
30 - 300
40
40@250A, 26V
208/230/460/575
1
60
POWER MIG® 350 MP
Chopper
Built-in
50 - 700
            
5 - 350
76
60@300A, 32V
208/230/460/575
1
50/60
Power Wave® S500
Inverter
External
                        
450
36.5
100
     
Power Wave® C300
Inverter
External
50 - 700
              
300
29
40
208/230/400/460/575
1/3
50/60
Power Wave® S350
Inverter
External
                  
350
31.5
40
208/230/380-415/460/575
1/3
50/60
Invertec® V350-PRO
Inverter
External
              
350
34
60
200-230/380-575
1/3
50/60

 MAGNATECH LLC East Granby, CT United States

MPS 4000
Inverter
On head, Push-pull
20 - 866
                      
400
70
50
200/230/460
3
50/60

 MILLER ELECTRIC MFG. CO. Appleton, WI United States

Millermatic 212
Tapped transformer
Built-in
50 - 700
                      
30 - 210
34.5
60@160A, 24.5V
208/230
1
60
Millermatic 350P
 
All-in-one
50 - 700
                    
25 - 400
32
60
200/230/410
3
60
Invision 352 MPa
Inverter
External
50 - 780
                    
350
34
60
208 - 575
3
60
XMT 350 CC/CV
Inverter
External
            
5-400
10-35
60@350A, 38 VDC
208/400/460/575
1/3
60
XMT 450 CC/CV
Inverter
External
            
5-600
10-38
100@450A, 38V
230/460/575
3
60
AlumaPower 350 MPa
Inverter
External
                        
5-425
10-38
60@350 A, 34 VDC
208-575
1/3
50/60
Deltaweld 452
Solid-state
External
                        
0 - 575
10 - 38
100@450A, 38V
200/230/460, 230/460/575
3
60
Millermatic 350P Aluminum
Inverter
All-in-one
50-800 IPM
                        
25 - 400
32
60@300A, 32 VDC
200/230/460, 230/460/575
1/3
60
Dimension 452
Solid-state
External
                    
20-565
10-38
100@450A, 38V
208/230/460, 460/575
3
60
CP302
Mechanical voltage control
External
                          
50-375
14-44
100@300A, 32V
208/230/460
3
60

 NU-TEC SYSTEMS LLC Gurnee, IL United States

MG130
Rectifier
Internal
30-300
                        
30-120
18.5
20@80A
120
1
50/60
MG140
Rectifier
Internal/Spool Gun
25-300
                        
30-140
19
30@90A
120
1
50/60
MG170
Rectifier
Internal/Spool Gun
40-500
                        
30-180
20
30@130A
208/240
1
50/60
MG260D
Rectifier
Internal/Spool Gun
40-700
                       
30-260
26.5
60@200A
208/240
1
50/60

 PANASONIC FACTORY SOLUTIONS CO. Rolling Meadows, IL United States

GBII-350
Inverter
External
50 - 750
                      
35 - 350
36
60@350A
460
3
60
HMIII-350
Inverter
External
50 - 750
                    
35 - 350
36
60@350A
230/460
3
60
HM3-500
Inverter
External
50 - 750
                    
40 - 500
45
100@500A
460
3
60