Robotic Welding Workcell Buyers' Guide©

Workcell Robot(s)
Robot
Reach
Positioner Type* No. of
Axes
Positioner
Load
Capacity
per Side
Workcell
Footprint
Welding Process PC Based Software Maximum
Part/Tool Size
Robot External GMAW GTAW Laser Spot Plasma FCAW

 Hot Link - TRUMPF Inc. - RoboticWelding TRUMPF INC. Farmington, CT United States   Email Icon - TRUMPF Inc. - RoboticWelding Video Icon - TRUMPF Inc. - RoboticWelding

TruLaser Cell 7040 TRUMPF Multiaxis 160 x 60(80) x 30 To spec. 5 1 1,764              
TruLaser Cell 7020 TRUMPF Multiaxis 80 x 60(80) x 30 To spec. 5 1 1,764              
TruLaser Cell 7006 Powertrain TRUMPF Multiaxis 26 x 80 x 30 To spec. 5 1 To spec. 240 x 282 x 150           To spec.
TruLaserCell 1100 TRUMPF Multiaxis 11.8 x 11.8 To spec. 2 2 To spec. 250 x 155 x 107.5              
TruLaser Cell 3000 TRUMPF Multiaxis 31, 24, 16   5   209.4 62.4 x 111.6 x 104.4            
TruLaser Robot 5020 KUKA KRC4 80 To spec. 6 1 551 352x230 (with resonator and chiller)             To spec.

 ABB INC. Auburn Hills, MI United States

ArcPack Lean 1410 IRB 1410 .057 To spec. 6 Up to 3 To spec.      
FlexArc 500C Single IRB 1600 .047-.057 IRBP 500C 6 3 500 17.4 x 11.8 x 8.2    
FlexArc 500C Multimove IRB 1600 (2) .047-.057 IRBP 500C 6 3 1,102 17.4 x 11.8 x 8.2    
FlexArc 250R Single IRB 1600 .047-.057 IRBP 250R 6 3 551 17.4 x 11.8 x 8.2    
FlexArc 250R Multimove IRB 1600 (2) .047-.057 IRBP 250R 6 3 551 17.4 x 11.8 x 8.2    
FlexArc 500R Single IRB 1600 .047-.057 IRBP 500R 6 3 1,102 22 x 12.1 x 8.2    
FlexArc 750R Single IRB 1600 .047-.057 IRBP 750R 6 3 1,653 22 x 12.1 x 8.2    
FlexArc 250K Single IRB 1600 .047-.057 IRBP 250K 6 3 551 18 x 14.1 x 8.2    
FlexArc 500K Single IRB 1600 .047-.057 IRBP 500K 6 3 1,102 19.7 x 17.4 x 9.8    
FlexArc 750K Single IRB 1600 .047-.057 IRBP 750K 6 3 1,653 19.7 x 17.4 x 9.8    

 FANUC ROBOTICS AMERICA CORP. Rochester Hills, MI United States

ARC Mate 50iC/5L ARC Mate 50iC/5L 35.1 HS, 2-axis positioner; to spec. Multiple Multiple 1,102/2,205/3,307 To spec. To spec.
ARC Mate 100iC/10S ARC Mate 100iC/10S 43.2 HS, 2-axis positioner; to spec. Multiple Multiple 1,102/2,205/3,307 To spec. To spec.
ARC Mate 100iC ARC Mate 100iC 55.9 HS, 2-axis positioner; to spec. Multiple Multiple 1,102/2,205/3,307 To spec. To spec.
ARC Mate 100iC/6L ARC Mate 100iC/6L 63.8 HS, 2-axis positioner; to spec. Multiple Multiple 1,102/2,205/3,307 To spec. To spec.
ARC Mate 120iC ARC Mate 120iC 71.3 HS, 2-axis positioner; to spec. Multiple Multiple 1,102/2,205/3,307 To spec. To spec.
ARC Mate 120iC/10L ARC Mate 120iC/10L 79.1 HS, 2-axis positioner; to spec. Multiple Multiple 1,102/2,205/3,307 To spec. To spec.
ARC Mate 100iCe ARC Mate 100iCe 55.9 Fixed T     To spec. To spec. To spec.
M710iC/20L-SA M710iC/20L-SA 122.4 HS, 2-axis positioner; to spec. Multiple Multiple 1,102/2,205/3,307 To spec. To spec.

 IGM ROBOTIC SYSTEMS INC. Menomonee Falls, WI United States

RST Rti 456, Rti 478, Rti 499 59.1, 66.9, 102.4 RP HS or RWM2 Skyhook 6, 7, 8 1- 5 22,000 To spec.         To spec.
RSH, RTSV, DM Rti 476, Rti 497 66.9, 74.8 HS or L-Arm 6, 7 3-7 44,000 To spec.         To spec.
TLA3 Rti 496 74.8 HS or L-Arm 6, 7 3-7 50 tons To spec.         To spec.
P2W -10 RTe 456 59 Single axis 6 1 400-2,000 To spec.       36x36
P2W-20 RTi 476 66.9 HS/TS 6 3 2,200 To spec.       28x59
P2W-30 RTi 476 or 496 66.9 or 74.8 2 axis tilt/rotate 6 5 330-2,200 To spec.       To spec.
RRMK-1002 RTi 456, 476, 496 59, 66, 74 HS/TS 6 -8 3 1,320-2,200 To spec.       48x118
RSX 502/1002 RTi 476 66.9 2 axis skyhook 2 stations 6-9 5 1,100-2,200 To spec.       To spec.

 LIBURDI AUTOMATION INC. Dundas, ON Canada

LAWS 445, 645, 800, 1000 FANUC 24 x 36 x 18 Vision-based compensation (+/-.002) 6 Up to 10 Var. 4 x 4 x 7         2 x 2 - 3 x 4

 LINCOLN ELECTRIC AUTOMATION Cleveland, OH United States

System 5 FANUC ARC Mate 100iC 55.9   6   2,500 69 x 123       24 x 70
System 10 FANUC ARC Mate 100iC 55.9   6   2,500 69 x 127       (2) 37x35
System 15 FANUC ARC Mate 50iC/5L 35.11   6   400 62.5 x 89       52
System 20 FANUC ARC Mate 100iC 55.9   6   600 126 x 84         58
System 35 FANUC ARC Mate 100iC 55.9   6   2,500 154 x 137       (2) 78x39
System 30 FANUC ARC Mate 100iC 55.9   6   2,500 80 x 181       (2) 36x42
System 30HS FANUC ARC Mate 100iC 55.9   6   2,000 - 6,000 80 x 181       30 x 30
System 40 FANUC ARC Mate 100iC 55.9   6   800 86 x 148.5       76
System 50HP FANUC ARC Mate 100iC 55.9   6   2,000-6,000 82 x 188       40 x 54
System 55 FANUC ARC Mate iC Family To spec. As needed 6   2,000-6,000 To spec.       36-72 x 84-144

 LINCOLN ELECTRIC CO., THE Cleveland, OH United States

Robotic Welding Education Cell FANUC ARC Mate 50iC/5L     6     81 x 64 x 66 (sides expanded)            

 OTC DAIHEN INC. Tipp City, OH United States

ECO-ARC 200 FD-V6, FD-B4 55 2 static tables 6 0 550 86.4 x 84.6 x 135     31.5 x 23.6/side
ECO-ARC 200L FD-V6L, FD-B4L 79 2 static tables 6 0 550 133.6 x 84.6 x 160     48 x 36/side
PT-ARC 600 FD-V6, FD-B4 55 60 pneumatic TT 6 0 550 86.4 x 88.0 x 180.5     60 x 30
SERVO-ARC 600 FD-V6, FD-B4 55 60 servo TT 6 1 550 86.4 x 88.0 x 180.5     60 x 30
SERVO-ARC 720 FD-V6, FD-B4, FD-V6L, FD-B4L 55, 79 72 servo TT 6 1 550 86.4 x 88.0 x 180.5     72 x 36
ROTA-ARC 1000 FD-V6, FD-B4, FD-V6L, FD-B4L 55, 79 Dual servo HS indexing H frame 6 3 2,200 133.8 x 86.6 x 240.7     59.06 x 39.37
TRI-ARC 500 FD-V6, FD-B4, FD-V6L, FD-B4L 55, 79 Dual servo HS indexing FW 6 3 1,100 246.4 x 120 x 225.8     137.79 x 41.34
TRI-ARC 1000 FD-V6, FD-B4, FD-V6L, FD-B4L 55, 79 Dual servo HS indexing FW 6 3 2,200 246.4 x 120 x 225.8     137.79 x 41.34
DT-ARC 500 FD-V6, FD-B4, FD-V6L, FD-B4L 55, 79 Dual servo HS/TS 6 2 1,100 165 x 93 x 227     78.7 x 39.37
DT-ARC 1000 FD-V6, FD-B4, FD-V6L, FD-B4L 55, 79 Dual servo HS/TS 6 2 2,200 165 x 93 x 227     78.7 x 39.37

 TAYLOR-WINFIELD TECHNOLOGIES Youngstown, OH United States

Custom To spec. To spec. To spec. To spec. To spec. To spec. To spec. To spec.

 TEC WELD AUTOMATION INC. Newton, KS United States

TecArc180 Motoman, Fanuc, ABB To spec. Floor TT 6/7 To spec. 500/1,000 To spec.   To spec.
TecArc 3 XT/HR Motoman, Fanuc, ABB Var. 3-axis horizontal rotation with 2 HS/TS 6/7 To spec. 500/1,500 To spec.   To spec.
TecArc Gantry Motoman, Fanuc, ABB To spec. Overhead Gantry with Dual HS/TS 6/7 To spec. 1,000-15,000 To spec.   To spec.
TecArc 5 XTR Motoman, Fanuc, ABB To spec. 5-axis Tilt & Rotate with Sweep 6/7 To spec. 500 -1,500 To spec.   To spec.
TecArc DHSTS Motoman, Fanuc, ABB To spec. Dual HS/TS 6/7 To spec. 500 - 10,000 To spec.   To spec.
TecArc Custom Cell Motoman, Fanuc, ABB To spec. To spec. 6/7 To spec. To spec. To spec.   To spec.
TecArc FTP Motoman, Fanuc, ABB To spec. Dual HS/TS, Floor Transport 6/7 To spec. 500 - 10,000 To spec.   To spec.

 TEST CO. Rockford, IL United States

Apple-24 1 1 1 1                

 WESTWOOD MANUFACTURING INC. Elizabethtown, NC United States

Auto-Shuttle/Auto Table/Flex ARCS ABB/Kuka 118 Servo positioners 6 7 165 Various       Various

 WORKER AUTOMATION INC. Covington, OH United States

ePRO® II Dual Table OTC 55, 79 Stationary T 6 0 1,000 7.3 x 11.1     32 x 40
ARCWORKER® ET-60, 72, 84 OTC 55, 79 TT 6 0 500 - 1,000 7.5 x 15   29 x 32
ARCWORKER® 2H OTC 55, 79 2 HS/TS 6 2 500 - 5,500 15 x 15.5   86 x 192
ARCWORKER® 3S OTC 55, 79 2 HS/TS on TT 6 3 500 - 4,000 7.6 x 10   60 x 88
ARCWORKER® Dual TR OTC 55, 79 Tilt & Rotate 6 4 660 - 8,000 7.6 x 14.8   48 x 48
LASERWORKER® OTC 55+ Many 6 0 To spec. To spec.           To spec.
ARCWORKER® 5S OTC 55, 79 5-axis 6 5 500 - 2,500 13 x 18   60 x 80
ARCWORKER® FW OTC 55, 79 FW 6 3 500 - 4,000 10 x 12   52 x 144
ARCWORKER® Dual Robots (opt.) OTC 55, 79 TT 6 0 500-4,000/750-4,000 To spec.   To spec.
Swing Arm & Gantry OTC 55, 79 To spec. 6 4 To spec. To spec.   To spec.

 YASKAWA AMERICA, INC. Miamisburg, OH United States

ArcWorld C/ArcWorld II-50 Series MA1400, VA1400   F, RT 6, 7 1 or 2 396     21.65 x 27.55, 51.18 x 27.55 dia.
ArcWorld II-200/500 Series MA1400, VA1400   F, RT 6, 7 1 or 2 1,212       39.37 x 31.49 dia.
AWC-500 Series MA1400, VA1400   F, RT, T/R 6, 7 2 or 4 2,369       51.18 x 43.30 dia
Arcworld 1000 MA1400, VA1400   TT 6, 7, 12, 14 0 661, 1,102     39.37 x 25.59
ArcWorld IV-4000 MA1400, MA1900   TT, RT 6, 12 3 1,102, 1,653       78.74 x 51.18 dia.
ArcWorld IV-6000SL MA1400, VA1400, MA1900   FW 6, 12, 18, 24; 7, 14, 21 3 551, 1,653     78.74, 118.11 x 51.18 dia.
ArcWorld IV-6000XHD MA1400, VA1400, MA1900   FW 6, 12, 18, 24; 7, 14, 21 3 2,645       118.11 x 51.18 dia.
ArcWorld V-6000 MA1400, VA1400, MA1900   FW 6, 12, 18, 24; 7, 14, 21 3 2,645     118.11 x 51.18 dia.
FabWorld, FabWorld II MA1900 (1 or 2); MA3100 74.80, 122.04 RT 6, 12 2 2,369, 6,613, 13,888         118.11 x 51.18, 157.48 x 78.74 dia.