Model or Series Electron Beam ERW High frequency Contact ERW High frequency Induction ERW Rotary Wheel Direct Current DC ERW Rotary Wheel Square Wave Laser Plasma Spiral Welding TIG GTAW OD Minimum Inches OD Maximum Inches Wall Thickness Minimum Inches Wall Thickness Maximum Inches Mild Steel Stainless Steel Aluminum Copper Other Metals Round Square Rectangle Other Shapes

 ADDISON MACHINE ENGINEERING INC. Reedsburg, WI United States

AM-050             .125 .500 .005 .030
AM-075             .188 .750 .007 .035
AM-1000     .250 1.000 .010 .049
AM-1500     .250 1.500 .015 .065
AM-1500X     .375 1.750 .020 .083
AM-2000     .500 2.250 .025 .125
AM-2500     .750 3.000 .030 .160
AM-3000       1.000 4.000 .040 .200
AM-4000     1.250 5.000 .050 .250
AM-4500     1.500 5.500 .060 .300
AM-5000     1.750 6.000 .075 .335
AM-6000     2.000 7.625 .090 .375

 CROWN HOLLANDER MACHINERY INC. Toronto, ON Canada

Spiral Pipe Mill                 416 120 .250 1                

 DREISTERN INC. Telford, PA United States

RSD 50               .25 2.00 .006 .016
RS 060             .118 1.00 .006 .040
RS 080             .118 1.50 .012 .040
RS 100     .40 2.00 .016 .078
RS 125     .55 3.00 .020 .102
RS 160     .71 4.00 .024 .142
RS 200     1.18 6.60 .028 .200

 EMMEDI - SAET GROUP Leinì (Torino), Italy

Vacuum Tube High-Frequency Welder               .31 24 .005 .63
Solid-State High-Frequency Welder               .31 24 .005 .63

 FIVES BRONX - ABBEY PRODUCTS North Canton, OH United States

1K-1.5             .375 1.5 .018 .083      
2X-2.25             .500 2.25 .020 .095    
2K-3.5             .625 3.5 .028 .125    
3X-3.5             .750 3.5 .032 .160    
3K-3.5               .840 3.5 .042 .203    
4X-5.0             1.25 5.0 .42 .188    
4K4.5               1.0 4.5 .049 .25    
5K-5.625                 1.25 5.625 .049 .25        
6X6.625             1.9 6.625 .049 .237      
6K-6.625                 1.9 6.625 .083 .338        
7X-7.5                 2.375 7.5 .065 .280        
7K-7.5                 2.375 7.5 .083 .340        
8K-8.75               2.875 8.75 .083 .375        
12X-12.75               3.5 12.75 .083 .330        
12K-12.75               3.5 12.75 .12 .625          
16K-16.0               4.5 16.0 .12 .625          
20K-20.0               6.625 20.0 .120 .5          
24K-24.0               8.625 24.0 .188 .750          
27K-27.0               10.75 27.0 .2 .750          
36K-30.0               14.0 36.0 .2 1.0          

 KENT CORP. North Royalton, OH United States

MTM 040 C             .240 1.110 .010 .047    
MTM 040 C Broom Handles                 .400 1.110 .008 .024              
MTM 040 C Window                 .22 x .260 1.20 x .260 .008 .020              
MTM 040 C Wire                   .100 .150 .020 .033            
MTM 040 Radiator - Intercoolers                 .7 x .60 1.50 x .1 .008 .047              
MTM 050 C             .400 1.500 .020 .098    
MTM 060 C             .500 2.500 .024 .120    
MTM 070 C             .630 3.000 .035 .157    
MTM 080 C               .830 3.150 .040 .197    
MTM 090 C               1.000 3.500 .040 .217    
MTM 100 C               1.300 4.500 .050 .217    
MTM 120 C               1.660 5.000 .060 .236      
MTM 130 C               2.500 6.620 .060 .276      
MTM 160 C               3.500 8.630 .079 .315        
MTM 170 C ST HF                 4.500 10.000 .100 .315          

 LIBURDI AUTOMATION INC. Dundas, ON Canada

Pulsweld LTP200-1200               .125 6 .020 .125  
WinTube Laser Mill                 .250 4 .010 .125      

 MILL MASTERS INC. Jackson, TN United States

Spectrum Series S-626                 .24 1.02 .010 .040
Spectrum Series S-1976                 .75 3.00 .015 .118
Premier Series P-626-T               .24 1.02 .010 .040
Premier Series P-19115T               .75 4.50 .015 .118
Elite Series E-1234 (Flat Oval)                 .47 1.35 .010 .025      
Elite Series E-1485 (Flat Oval)                 .56 3.34 .012 .040      

 NAKATA MANUFACTURING CO. LTD. Osaka, Osaka Japan

FFX             2 26 .031 1.000        

 RAFTER EQUIPMENT CORP. Strongsville, OH United States

RT-1000             .250 1.000 .010 .049      
RT-1250             .250 1.250 .020 .065    
RT-1500           .375 1.750 .020 .083    
RT-2000           .500 2.500 .020 .120    
RT-2000S           .500 3.000 .028 .135    
RT-2500           .075 3.000 .032 .165    
RT-3000           .750 4.000 .032 .188    
RT-3500           1.000 5.000 .048 .250      
RT-4500           1.250 6.000 .060 .300      
RT-6000           2.500 8.625 .065 .440      
RT-8000               4.000 12.750 .065 .500      
RT-9000               6.625 16.000 .120 .625      

 SEUTHE GMBH Hemer, Germany

Conventional RS 16               .185 .630 .019 .060      
Conventional RS 30               .394 1.181 .024 .160      
Conventional RS 60               .630 2.362 .035 .250      
Conventional RS 127               1.496 5.000 .059 .320      
Conventional RS 168               1.902 6.626 .079 .400    
Conventional RS 273               2.996 10.748 .118 .500    
Conventional RS 406               5.551 15.984 .157 .625    
Conventional RSE 25         .250 1.000 .020 .100        
Conventional RSE 60         .625 2.375 .028 .118        
Conventional RSE 127         1.500 5.000 .040 .250        
Cage Forming 90 Round               1.625 3.500   .177    
Cage Forming 127 Round               1.900 5.000   .250    
Cage Forming 168 Round               2.375 6.625   .315    
Cage Forming 220 Round               3.000 8.625   .375    
Cage Forming 406 Round               5.500 16.000   .625    
Cage Forming 240 Square               .750 x .750 2.375 x 2.375   .125      
Cage Forming 400 Square               1.500 x 1.500 4.000 x 4.000   .250      
Cage Forming 600 Square               2.375 x 2.375 6.000 x 6.000   .312      
Cage Forming 1000 Square               4.000 x 4.000 9.875 x 9.875   .500      
Cage Forming 1600 Square               5.875 x 5.875 15.750 x 15.750   .625      

 T & H LEMONT INC. Countryside, IL United States

WU-8               .090 .375 .006 .035      
WU-11           .150 .750 .010 .050
WU-11M           .250 1.000 .020 .065
WU-15           .375 1.750 .020 .083
WU-20           .500 2.500 .020 .134
WU-25         .750 3.500 .025 .160
WU-35         1.000 4.500 .060 .240
WU-40         1.500 5.500 .060 .280
WU-50         2.000 6.625 .080 .330
WU-60         2.000 8.625 .110 .375

 THERMATOOL CORP. East Haven, CT United States

              .125 24.0 .010 1.0

 UNIVERSAL TUBE & ROLLFORM EQUIPMENT CORP. Perrysburg, OH United States

190-6                 2.362 7.480   .240        

 YODER - A MEMBER OF THE FORMTEK GROUP Cleveland, OH United States

12" Pipe Mill               4.500 12.750 .083 .625
16" Pipe Mill               4.500 16 .120 .625
26" Pipe Mill               6.625 28 .120 1.000
6" Pipe Mill               2.375 6.625 .065 .438
8" Pipe Mill               2.875 8.625 .083 .500
M-1-1/2 & QVW-150       .313 1.250 .018 .049
M-2 & QVW-200       .500 2.250 .018 .095
M-2-1/2 & QVW-250       .500 3 .018 .134
W-10S/W-15S       .188 .500 .020 .040
WH-150       .375 1.500 .020 .083
WH-200       .500 3.000 .020 .135
WH-250       .750 3.500 .035 .180
WH-350       1.250 5.500 .065 .375