- FMA
- The Fabricator
- FABTECH
- Canadian Metalworking
Our Publications
Categories
- Additive Manufacturing
- Aluminum Welding
- Arc Welding
- Assembly and Joining
- Automation and Robotics
- Bending and Forming
- Consumables
- Cutting and Weld Prep
- Electric Vehicles
- En Español
- Finishing
- Hydroforming
- Laser Cutting
- Laser Welding
- Machining
- Manufacturing Software
- Materials Handling
- Metals/Materials
- Oxyfuel Cutting
- Plasma Cutting
- Power Tools
- Punching and Other Holemaking
- Roll Forming
- Safety
- Sawing
- Shearing
- Shop Management
- Testing and Measuring
- Tube and Pipe Fabrication
- Tube and Pipe Production
- Waterjet Cutting
Industry Directory
Webcasts
Podcasts
FAB 40
Advertise
Subscribe
Account Login
Search
Covestro introduces 3D printing material made from recycled plastic
- May 12, 2021
- Product Release
- Additive Manufacturing
Polymers manufacturer Covestro AG has introduced Arnite AM2001 GF (G), a recycled polyethylene terephthalate (rPET) for pellet-style 3D printers. The company says the material, made from used consumer products, supports its corporate goal of developing sustainable products.
The glass-fiber-filled material enhances the structural performance of parts while leaving a smaller carbon footprint than virgin material, according to Covestro. The material has been optimized for 3D pellet printing. The technology, also known as fused granulate fabrication, is designed to allow fast, economical printing of large parts.
Covestro recommends rPET for structural applications, including pedestrian bridges, tiles for cyclist or pedestrian tunnels, architectural applications like cladding or partition walls, indoor and outdoor furniture, small boats, and packaging crates.
rPET is the first 3D printing material from Royal DSM’s Resins & Functional Materials business, which Covestro acquired April 1.
- Podcasting
- Podcast:
- The Fabricator Podcast
- Published:
- 04/30/2024
- Running Time:
- 53:00
Seth Feldman of Iowa-based Wertzbaugher Services joins The Fabricator Podcast to offer his take as a Gen Zer...
- Trending Articles
- Industry Events
Pipe and Tube Conference
- May 21 - 22, 2024
- Omaha, NE
World-Class Roll Forming Workshop
- June 5 - 6, 2024
- Louisville, KY
Advanced Laser Application Workshop
- June 25 - 27, 2024
- Novi, MI
Precision Press Brake Certificate Course
- July 31 - August 1, 2024
- Elgin,