- FMA
- The Fabricator
- FABTECH
- Canadian Metalworking
Our Publications
Categories
- Additive Manufacturing
- Aluminum Welding
- Arc Welding
- Assembly and Joining
- Automation and Robotics
- Bending and Forming
- Consumables
- Cutting and Weld Prep
- Electric Vehicles
- En Español
- Finishing
- Hydroforming
- Laser Cutting
- Laser Welding
- Machining
- Manufacturing Software
- Materials Handling
- Metals/Materials
- Oxyfuel Cutting
- Plasma Cutting
- Power Tools
- Punching and Other Holemaking
- Roll Forming
- Safety
- Sawing
- Shearing
- Shop Management
- Testing and Measuring
- Tube and Pipe Fabrication
- Tube and Pipe Production
- Waterjet Cutting
Industry Directory
Webcasts
Podcasts
FAB 40
Advertise
Subscribe
Account Login
Search
Thermo Scientific Explorer 4 Additive SEM delivers 3-D printing process control
- May 8, 2018
- Product Release
- Additive Manufacturing
The new Thermo Scientific Explorer 4 Additive is the first commercially released SEM designed to measure particle size, shape, and composition in AM metal powders and to inspect finished parts to ensure quality, says the company.
The SEM automatically and simultaneously analyzes particle size distribution and morphology. Advanced energy-dispersive X-ray (EDX) spectrometry provides fast elemental analysis that can automatically identify impurities. Suspect particles can be relocated for more detailed examination.
The system’s ability to examine and classify large sets of particles, inclusions, voids, and cracks within minutes enables the use of SPC techniques and permits faster responses to process excursions, the manufacturer reports.
Related Companies
- Podcasting
- Podcast:
- The Fabricator Podcast
- Published:
- 05/14/2024
- Running Time:
- 62:12
Cameron Adams of Laser Precision, a contract metal fabricator in the Chicago area, joins the podcast to talk...
- Trending Articles
- Industry Events
Laser Welding Certificate Course
- May 7 - August 6, 2024
- Farmington Hills, IL
World-Class Roll Forming Workshop
- June 5 - 6, 2024
- Louisville, KY
Advanced Laser Application Workshop
- June 25 - 27, 2024
- Novi, MI
Precision Press Brake Certificate Course
- July 31 - August 1, 2024
- Elgin,