Herr-Voss Stamco manufacturing slitting line for Cascadia Metals


October 23, 2013

Herr-Voss Stamco, Callery, Pa., is manufacturing a new Strand Extensioner® slitting line for Cascadia Metals Ltd., Brandon, Man.

The line will process material with a thickness of 0.012 to 0.25 in. with an incoming coil capacity of 50,000 lbs. by 72 in. wide. The slitting line also includes a quick-change injector slitter head system that allows operators to change slitter heads out of the line.