- FMA
- The Fabricator
- FABTECH
- Canadian Metalworking
Categories
- Additive Manufacturing
- Aluminum Welding
- Arc Welding
- Assembly and Joining
- Automation and Robotics
- Bending and Forming
- Consumables
- Cutting and Weld Prep
- Electric Vehicles
- En Español
- Finishing
- Hydroforming
- Laser Cutting
- Laser Welding
- Machining
- Manufacturing Software
- Materials Handling
- Metals/Materials
- Oxyfuel Cutting
- Plasma Cutting
- Power Tools
- Punching and Other Holemaking
- Roll Forming
- Safety
- Sawing
- Shearing
- Shop Management
- Testing and Measuring
- Tube and Pipe Fabrication
- Tube and Pipe Production
- Waterjet Cutting
Industry Directory
Webcasts
Podcasts
FAB 40
Advertise
Subscribe
Account Login
Search
Henkel, Clemson University develop methods to measure thermal expansion in multisubstrate assemblies
- March 28, 2017
- News Release
- Assembly and Joining
Henkel, a Madison Heights, Mich.-based provider of adhesives, sealants, and surface treatments for the automotive industry, in cooperation with Clemson University – International Center for Automotive Research (CU-ICAR) in Greenville, S.C., has announced the development of novel experimental methodologies used to measure thermal expansion for dissimilar substrates used in vehicle development. Thermal expansion, which measures the substrate growth during heating, presents a significant challenge for automotive engineers, particularly as new lightweight materials are introduced.
"When one substrate grows faster than another during heating, potential issues can arise, including distortion, adhesive stress, and potential debonding of adhesive joints," said Michael Flener, innovation program manager, transportation and metals industries, Henkel. "By using these experimental methods in conjunction with our predictive models, OEMs can better determine the ideal location and types of joining areas needed during the vehicle design and development process."
The developed experimental methodologies use noncontact optical measurement systems that were customized and further developed to allow measurements at cold and high temperatures through oven windows. The developed methodologies have been validated through accurate measurements of thermal expansion and material deformation in coupon-level samples, subassemblies, and even large full-scale vehicles.
"These methods can measure full-field thermal expansion within one-tenth of a millimeter of accuracy,” said Fadi Abu-Farha, assistant professor, automotive engineering, CU-ICAR, “resulting in data that provide highly accurate understanding of how substrates and adhesives are interacting within automotive thermal cycles."
subscribe now
The Fabricator is North America's leading magazine for the metal forming and fabricating industry. The magazine delivers the news, technical articles, and case histories that enable fabricators to do their jobs more efficiently. The Fabricator has served the industry since 1970.
start your free subscription- Stay connected from anywhere
Easily access valuable industry resources now with full access to the digital edition of The Fabricator.
Easily access valuable industry resources now with full access to the digital edition of The Welder.
Easily access valuable industry resources now with full access to the digital edition of The Tube and Pipe Journal.
Easily access valuable industry resources now with full access to the digital edition of The Fabricator en Español.
- Podcasting
- Podcast:
- The Fabricator Podcast
- Published:
- 04/30/2024
- Running Time:
- 53:00
Seth Feldman of Iowa-based Wertzbaugher Services joins The Fabricator Podcast to offer his take as a Gen Zer...
- Industry Events
Pipe and Tube Conference
- May 21 - 22, 2024
- Omaha, NE
World-Class Roll Forming Workshop
- June 5 - 6, 2024
- Louisville, KY
Advanced Laser Application Workshop
- June 25 - 27, 2024
- Novi, MI
Precision Press Brake Certificate Course
- July 31 - August 1, 2024
- Elgin,