- FMA
- The Fabricator
- FABTECH
- Canadian Metalworking
Categories
- Additive Manufacturing
- Aluminum Welding
- Arc Welding
- Assembly and Joining
- Automation and Robotics
- Bending and Forming
- Consumables
- Cutting and Weld Prep
- Electric Vehicles
- En Español
- Finishing
- Hydroforming
- Laser Cutting
- Laser Welding
- Machining
- Manufacturing Software
- Materials Handling
- Metals/Materials
- Oxyfuel Cutting
- Plasma Cutting
- Power Tools
- Punching and Other Holemaking
- Roll Forming
- Safety
- Sawing
- Shearing
- Shop Management
- Testing and Measuring
- Tube and Pipe Fabrication
- Tube and Pipe Production
- Waterjet Cutting
Industry Directory
Webcasts
Podcasts
FAB 40
Advertise
Subscribe
Account Login
Search
Dry ice blast cleaning process safely removes grease, sludge, sealants, weld slag
- October 10, 2006
- Product Release
- Finishing
Cold Jet offers a dry ice blasting system that the manufacturer says is an efficient and environmentally safe process for the removal of excessive grease, sludge, sealants, and weld slag from production equipment.
The process uses solid CO2 media and thermal shock and kinetic energy to blast contaminants from surfaces. As the dry ice (-78.5 degrees C) blasts against the surface, the contaminant loses its adhesion. The warmer temperature of the surface causes the solid CO2 to revert back to gas, leaving no secondary waste and expanding underneath the contaminant, allowing it to break free.
It uses compressed air between 80 and 100 PSIG and the dry ice to create a blast stream that does not affect the equipment, solenoids, fittings, wiring harnesses, or electrical circuitry.
Related Companies
subscribe now
The Fabricator is North America's leading magazine for the metal forming and fabricating industry. The magazine delivers the news, technical articles, and case histories that enable fabricators to do their jobs more efficiently. The Fabricator has served the industry since 1970.
start your free subscription- Stay connected from anywhere
Easily access valuable industry resources now with full access to the digital edition of The Fabricator.
Easily access valuable industry resources now with full access to the digital edition of The Welder.
Easily access valuable industry resources now with full access to the digital edition of The Tube and Pipe Journal.
Easily access valuable industry resources now with full access to the digital edition of The Fabricator en Español.
- Podcasting
- Podcast:
- The Fabricator Podcast
- Published:
- 05/14/2024
- Running Time:
- 62:12
Cameron Adams of Laser Precision, a contract metal fabricator in the Chicago area, joins the podcast to talk...
- Trending Articles
White House considers China tariff increases on materials
A visit to Automate 2024 reveals the future might be now
Majestic Steel Arkansas fully operational
Why employee-owned companies make sense in manufacturing
Rivian to expand Illinois facility to manufacture midsized SUV
- Industry Events
Laser Welding Certificate Course
- May 7 - August 6, 2024
- Farmington Hills, IL
World-Class Roll Forming Workshop
- June 5 - 6, 2024
- Louisville, KY
Advanced Laser Application Workshop
- June 25 - 27, 2024
- Novi, MI
Precision Press Brake Certificate Course
- July 31 - August 1, 2024
- Elgin,